The microstructure and mechanical properties of Hastelloy B and its wear behavior against graphite in a simulated mechanical face seal
Hastelloy B is a commercial nickel-28 weight percent molybdenum-five weight percent iron-0.05 weight percent carbon alloy. The microstructures and the mechanical properties of Hastelloy B were studied, and its wear behavior against the graphite (grade SK217B, manufactured by Stackpole Carbon Company) was investigated.
Tensile properties of Hastelloy B were measured from 25 to 871°C. In this condition, the alloy retained up to 750°C more than half of its strength at 25°C. The aging response of the solution annealed condition was studied from 705 to 900°C. The microstructure has been characterized and the tensile properties and hardness at 25°C have been measured for aging time up to l200 hours. The most prominant strengthening occurred at 705°C; for example, the hardness doubled in 1200 hours. At 815 and 900°C, a needle-like precipitate formed. At 705 and 760°C, a Widmanstätten precipitate and a featherlike precipitate formed.
Wear tests were run under conditions simulating the operation of a dry mechanical face seal. Argon was used as the sealant to minimize the chemical reactions. Values of mating pressure and rotational speed were chosen so that the wear tests were conducted in two regimes: (1) light wear regime, which was associated with a low load operation in which graphite lubrication dominated the wear reaction; (2) heavy wear regime, in which the wear rate was excessive as a result of overload, Two solution annealed rings and two rings age hardened at 705°C for 800 hours were tested against graphite rings in the two load regimes. Wear debris were collected during the tests to aid the identification of the wear mechanism.
Scanning electron microscopy was used to observe and characterize the surface topography. In the light wear tests, the formation of a degraded layer on the graphite and the transfer of graphite onto the metal surface was observed. The combination of Hastelloy B and the graphite was satisfactory for its low friction and wear in this solid lubrication condition. In the heavy wear tests, the severe wear seemed to be initiated by surface fatigue and then transformed to a combined mechanism of brittle fracture and abrasive ploughing. Age hardened ring of Hastelloy B showed better wear resistance than the solution annealed ring in the heavy wear tests. Irrespective of the great distinctions of the microstructures and mechanical properties between these two heat treatments, there was no obvious difference between the wear surface topography. The wear of Hastelloy B was due to an abrasive mechanism, which was attributed to the hard silicon carbide particles in the graphite.