An investigation of alloying effects in aluminum dispersion strengthened with A1
The purpose of this investigation was to determine the effects of alloying elements on the mechanical properties of aluminum dispersion strengthened by its own oxide, commonly referred to as sintered aluminum product (SAP). SAP is noted for its high strength at elevated temperatures compared to conventional aluminum alloys. However, it has seen little application due to its low ductility at high temperatures and its relatively low strength at room temperature compared to conventional aluminum alloys. Two types of alloying elements were investigated to determine if the room-temperature strength could be improved and if, through lowering the oxide content, the high-temperature ductility could be improved. Magnesium was investigated for its solid solution strengthening in one type alloy. The other type alloy involved further dispersion strengthening through adding the elements iron, molybdenum, zirconium, chromium, vanadium, and titanium which form highly stable intermetallic compounds with aluminum.
To evaluate the effects of the alloying, fabrication techniques were developed which produced uniform and reproducible rods for testing. Prealloyed powders were produced by atomizing the molten alloys and collecting the powders in water. This procedure produced uniform powders with a very fine distribution of the intermetallic compounds. Fabrication into rods then included ball-milling, vacuum hot pressing, vacuum heat treating, and hot extrusion.
The magnesium additions improved strengths up to 200°C with little effect above that temperature. Room-temperature tensile strengths up to 77,O00 psi were obtained which are comparable to the strengths obtained in conventional aluminum alloys. The additional dispersion strengthening of the intermetallic compounds is additive to that of the oxide from room temperature to 450°C. No significant improvements in ductility are obtained by reducing the oxide content since even at very low ball-milling times (i.e., low oxide contents) the uniform elongation at 450°C is typically O.5%. Good combinations of strength and ductility at 450°C were obtained in some of the alloys containing intermetallic compounds with no ball-milling. Typical properties at this temperature were tensile strengths of 7,O00 psi, uniform elongation of 3%, and total elongation of 35%.
Thesis75b.C668.pdf
18.68 MB
Adobe PDF
b643ee653b4fe3dbe9fabafa35286f5b