The effect of strain rate upon the morphology of high purity 26 per cent chromium-1 percent molybdenum ferritic stainless steel tubing
The response of thin wall 26 per cent chromium-1 per cent molybdenum ferritic stainless steel alloy tubular sections to high velocity impulse loading was investigated. The experimental data was compared to results obtained from impact-flattening drop weight testing on similar material and section size. The results showed that some tubular sections which exhibited completely ductile behavior at impact-flattening strain rates are subject to brittle characteristics when explosively impulse loaded. The effects of tube manufacturing method, heat treatment, and post heat treatment rotary straightening were found to be related to high velocity deformation behavior. Optical microscopy of tube sections, before and after deformation, is presented and correlated with the experimental data.