The solution fabrication and wet spinning of polyamides
Date Issued
December 1975
Author(s)
Hancock, Tony Alan
Advisor(s)
James L. White
Additional Advisor(s)
Edward Clark
Joe E. Spruiell
Abstract
Apparatus to carry out wet spinning was designed and built. Four polyamides were wet spun into fiber. The fiber structure was characterized and fiber mechanical properties were measured. The materials studied were Nylon-6, Nylon-66, and redissolved DuPont Nomex and Kevlar. The spinning conditions were varied over a range of dope concentrations, coagulation bath concentrations, and temperatures. The effects of polymer solvent on spinnability were also examined.The superstructure of the resulting wet spun fibers was studied using scanning electron micrographs and optical micrographs. These results were correlated to spinning conditions. The fibers were also examined using both small angle and wide angle x-ray diffraction.Nylon-6 and Nylon-66 wet spun fibers were crystalline in the α-forms as-spun. They were very porous fibers with low elongations to breakand low tensile strengths. The porosity of of the fiber increased with the increasing coagulation bath pH. Nomex fibers were more uniform and showed better physical properties then the aliphatic polyamides. Kevlar was crystalline and oriented as-spun from anistropic dopes, but it exhibited little orientation when spun from anistropic dopes decreased upon annealing or hot drawing.
Degree
Master of Science
Major
Chemical Engineering
File(s)![Thumbnail Image]()
Name
Thesis75.H252.pdf
Size
14.88 MB
Format
Adobe PDF
Checksum (MD5)
3e551137bd3dae466785d2a215dadcaf