  5. Interlaminar Hybridization of Woven CF/PEI Laminates Using Chip-Recovered Discontinuous Carbon Fiber Thermoplastic Matrix: Mechanical Performance and Characterization
Details

Interlaminar Hybridization of Woven CF/PEI Laminates Using Chip-Recovered Discontinuous Carbon Fiber Thermoplastic Matrix: Mechanical Performance and Characterization

Date Issued
August 2026
Author(s)
Miner, Jordan Alexander
The University of Tennessee
Advisor(s)
Uday Vaidy
Dustin Gilmer
Additional Advisor(s)
Krishnan Veluswamy
Permanent URI
https://trace.tennessee.edu/handle/20.500.14382/61620
Abstract
This study investigates a compression molding technique combining discontinuous carbon fiber reinforced polyetherimide (CF-PEI) matrices with woven fiber layups to create high fiber loading hybrid composites. Four commercially available PEI grades were used in this work; matrix material was obtained by vacuum collection of machining chips from a sacrificial part. Samples were manufactured using hand layup of alternating layers of CF-PEI chips and woven CF. The addition of discontinuous fiber was intended to increase the shear strength due to 3D random alignment of short fibers spanning between layers of woven carbon fiber. Characterization included thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), rheological assessment, optical microscopy, and interlaminar shear strength testing. The use of short fiber-loaded polymers and chip-based layups represent a novel pathway for composite manufacturing, with potential implications for structural performance, process efficiency, and material customization. At high woven fiber loading, the neat chip-based PEI laminates exhibited the highest short-beam strength among the chip-based matrices, while the film-stacked control performed worst at every layer count. At 23 and 20 woven layers, the SBS hierarchy followed A>B>C>F, with neat PEI outperforming the carbon-fiber-filled chip matrices. At 12 woven layers, this ranking reversed to C>B>A>F, and the 40 wt% CF-PEI chip-based laminate exhibited the highest SBS. This reversal is the principal finding of the study and indicates that the optimal interlaminar matrix depends on woven-to-matrix volume ratio: neat PEI is favored when the interply region is thin, whereas discontinuous-fiber-filled chip interlayers become advantageous when the interlaminar region is sufficiently large. Density, constituent-content, and microscopy results further showed that the 40 wt% chip-based laminates achieved the lowest porosity, consistent with the flake-like chip morphology and improved consolidation observed at low woven layer count.
Subjects

Composites

Thermoplastic Composi...

Degree
Master of Science
Major
Mechanical Engineering
Embargo Date
August 1, 2027

University Libraries

1015 Volunteer Boulevard
Knoxville, TN 37996
865-974-4351

Map & Directions
Donate to the Libraries
  • About
  • John C. Hodges Society
  • Speaking Volumes magazine
  • Outreach
  • Directory
  • Employment
  • Policies
  • Library Intranet
University of Tennessee power T logo

The University of Tennessee, Knoxville
Knoxville, Tennessee 37996
865-974-1000

Events
A-Z
Apply
Privacy
Map
Directory
Give to UT
Accessibility

Built with DSpace-CRIS software - Extension maintained and optimized by 4Science