Abstract

The purpose of this study was to experimentally investigate the effect of drawing variables, draw ratio, draw temperature and draw rate, on the microstructure and mechanical properties of polyoxymethylene fibers. The microstructure of the drawn filaments was characterized using scanning electron microscopy, wide angle x-ray diffraction, small angle x-ray scattering and thermal property measurements. The tensile properties which were examined included the elastic modulus, tensile strength and elongation to break.

A drawing system was designed and built to draw filament at an elevated temperature. The superdrawn fibers were formed by melt extrusion and subsequent two stage drawing at a controlled draw rate and drawing temperature. The first stage of drawing converted the initial spherulitic structure into a natural drawn fiber with a lamellar structure. The second stage drawing was slower and hence rate controlling. This two stage drawing process produced the filament with extended chain structure with isolated chain folding defects.

The superdrawn Delrin fibers produced using this two stage process showed elastic modulus of 25.2 GPa (3.65x106 psi), which is 47.5% of the maximum theoretical modulus. The tensile strength was 1.16 GPa (1.68x105 psi) and elongation at break was 2% for the superdrawn fiber. These fibers were produced at 140°C and draw rate of 4%/min (5 mm/mm).

The mechanical properties increased with the draw ratio. Although the draw rate did not have any effect on the properties, it was found that the filament broke if it was drawn at a rapid rate. The mechanical properties of superdrawn fiber varied with the drawing temperature. It was found that 140°C was the optimum drawing temperature for acetal fibers. Scanning electron micrographs showed thin ''ribbon" like microfibrils.

 At the optimum drawing temperature of 140°C, Celcon filaments were draw. The mechanical properties were compared with Delrin superdrawn filament. Celcon superdrawn fiber showed the highest modulus, of 21 GPa (3.05x106 psi). The tensile strength was comparatively lower than Delrin fibers.

The elastic modulus of the superdrawn acetal fibers, after annealing at 150°C for two hours, was found to reduce by 8.7%, while the tensile strength decreased by 9.8%. This indicated a thermally stable structure for superdrawn filaments. The same fact was also reflected in the shrinkage measurements. The superdrawn fiber showed shrinkage of about 1% after heating for one hour.

 
Degree
Master of Science
Major
Chemical Engineering
File(s)
Thumbnail Image
Name

Thesis76.J683.pdf

Size

8.73 MB

Format

Adobe PDF

Checksum (MD5)

04577800b4eeda0cce570218709246fb


University Libraries

1015 Volunteer Boulevard
Knoxville, TN 37996
865-974-4351

Map & Directions
Donate to the Libraries
  • About
  • John C. Hodges Society
  • Speaking Volumes magazine
  • Outreach
  • Directory
  • Employment
  • Policies
  • Library Intranet
University of Tennessee power T logo

The University of Tennessee, Knoxville
Knoxville, Tennessee 37996
865-974-1000

Events
A-Z
Apply
Privacy
Map
Directory
Give to UT
Accessibility

Built with DSpace-CRIS software - Extension maintained and optimized by 4Science