  5. The effect of melt spinning and drawing variables on the structure and mechanical properties of isotactic polypropylenes
Details

The effect of melt spinning and drawing variables on the structure and mechanical properties of isotactic polypropylenes

Date Issued
August 1976
Author(s)
Nadella, Hari P.
Advisor(s)
Joseph E. Spruiell
Additional Advisor(s)
J. L. White
E. S. Clark
Permanent URI
https://trace.tennessee.edu/handle/20.500.14382/60911
Abstract

The purpose of this experimental study was to investigate the effect of spinline and drawing variables on the structure and properties of isotactic polypropylene fibers. Hercules Profax® (6323, 6423, 6823) and Tennessee Eastman Tenite ® (4241, 4221) polypropylenes having a range of melt flow indices (0.42 - 12.0) were selected for the experimental study. These polypropylenes were melt spun under various spinning conditions at an extrusion temperature of 230°C. The structures of the spun filaments were characterized using wide angle x-ray diffraction, small angle x-ray scattering, birefringence and density measurements. The tensile mechanical properties were also measured for the spun filaments.

Selected fibers were drawn in an Instron tensile testing machine. Two drawing processes were examined; cold drawing followed by annealing at 140°c and hot drawing at 140°c. The structures and mechanical properties of the drawn fibers were also characterized.

The spinnability of the polypropylenes decreased with increased molecular weight and decreased flow rate. The structure of the spun filaments varied according to the spinline variables considered. Spinning polypropylene into cold water at low stresses resulted in a para-crystalline (smectic) structure, whereas spun samples spun into ambient air have a monoclinic crystal structure. For samples spun into air. the structure and morphology of the filaments could be correlated with the stress under which the crystallization occurred. Changes in variables which produced greater spinline stress such as increased take-up velocity, decreased extrusion rate, and increased molecular weight produced increases in both crystalline and amorphous orientation and a change from a spherulitic to a row nucleated morphology. The tensile strength and elastic modulus increased and the elongation to break decreased as the spinline stress increased.

The drawn fibers showed improvements in mechanical properties over the spun fibers. The hot-drawn fibers generally showed higher levels of birefringence (average molecular orientation) and slightly better mechanical properties than the cold drawn and annealed fibers. Under the experimental conditions investigated, the mechanical properties of the drawn fibers (both cold and hot drawn) correlated with the birefringence.

This correlation with birefringence was extended to include the spun fibers as well as the drawn filaments. It is significant that the correlation seemed valid independent of the molecular weight of the polymer and the spinning and/or drawing conditions.

 
Degree
Master of Science
Major
Chemical Engineering
File(s)
Thumbnail Image
Name

Thesis76.N234.pdf

Size

8.18 MB

Format

Adobe PDF

Checksum (MD5)

a336b3f92d1ea56f47dd628a38dc0f29


University Libraries

1015 Volunteer Boulevard
Knoxville, TN 37996
865-974-4351

Map & Directions
Donate to the Libraries
  • About
  • John C. Hodges Society
  • Speaking Volumes magazine
  • Outreach
  • Directory
  • Employment
  • Policies
  • Library Intranet
University of Tennessee power T logo

The University of Tennessee, Knoxville
Knoxville, Tennessee 37996
865-974-1000

Events
A-Z
Apply
Privacy
Map
Directory
Give to UT
Accessibility

Built with DSpace-CRIS software - Extension maintained and optimized by 4Science