A new class of polyolefin filament ; the superdrawing of polypropylene
The purpose of this experimental study was to investigate the effects of initial filament crystal structure, drawing variables and drawability on the microstructure and tensile properties of isotactic polypropylene filaments. The microstructure of the drawn filaments was characterized using scanning electron microscopy, wide-angle X-ray diffraction, and density and thermal property measurements. The tensile properties which were examined included the elastic modulus, tensile strength and elongation to break.
The superdrawn high-strength filaments were formed by melt extrusion of the initial filament followed by a twostep drawing mechanism at controlled drawing rates and temperatures. The first drawing step converted the initial filament with an unoriented spherulitic structure to the natural drawn filament with a lamellar structure. The subsequent drawing step (rate controlling) produced the superdrawn filament with a structure of integrated chain-folds in a crystalline matrix. The initial filament structures which were investigated were the monoclinic and the smectic forms which were used to determine the drawability and final properties of the ultimate superdrawn filaments formed from them.
Superdrawn polypropylene filaments which were produced in this research had the following outstanding mechanical properties: an elastic modulus of up to 22 GPa, tensilestrength of up to 1 GPa, and an elongation to break of 8%. Appropriate structural analysis resulted in revealing that the superdrawn filaments (drawn at 4%/min and 130°C) showed very little small-angle X-ray scattering on the equator and no scattering on the meridian. The superdrawn filament was found to have a c-axis orientation function of 0.99 and a crystallinity of 85%. The microstructure of this filament was found to contain no microvoids which were detectable by scanning electron microscopy and was found to contain no basic structural unit smaller than the microfibril with a diameter on the order of 100nm.
The mechanical properties were found to be dependent on the drawing rate and drawing temperature. At a drawing rate of 4%/min the superdrawn filaments originating from both the monoclinic structure and smectic structure had very similar mechanical properties, but at the higher drawing rates the superdrawn filament originating from the initial smectic filament obtained higher draw ratios and slightly higher moduli and tensile strengths.
The mechanical properties of the superdrawn filaments were also found to be dependent on the molecular weight and molecular weight distribution of the polypropylene resin. The filaments formed from the resin with the highest weight average molecular weight produced the highest tensile strength.