Durability of flame resistant children's sleepwear to use and laundering by typical consumer families
The objectives of this study were to evaluate the durability of children's flame resistant sleepwear with respect to consumer use and practices; and to determine the effect of laundering and wear on the care flame resistance of the garments, and on other physical properties. One hundred percent FR treated cotton pajamas for boys and polyester/ matrix blend gowns were purchased and distributed to wear study participants.
The majority of participants rated the garments average to excellent in all characteristics covered by the questionnaire. In the panel ratings, most garments were rated average to above average. In every characteristic, the pajamas were given higher ratings than the gowns, except both received the same rating for overall appearance.
The participants followed the manufacturer's care instructions closely. Most washed garments by machine in warm water, using low phosphate detergent and dried them in a dryer. Some of the participants used fabric softener. Only a few pajamas were washed with bleach which violated the instruction.
Yarn count of both gowns and pajamas increased after consumer use. The shrinkage of gowns varied considerably, but the pajamas had good dimensional stability in both filling and warp direction. For gowns, the fabric weight increased, and the fabric thickness decreased after they were worn and laundered. Both fabric weight and thickness decreased after the pajamas were used. The readings of air permeabilit of gowns reflect the measured changes in fabric weight. After gowns were used, the air permeability became lower. The air permeability of pajamas was higher because pajamas were thinner and lighter after consumer use. Laundering and wearing did have an effect on the bursting strength of the gowns but not for the pajamas. The bursting strength of the gowns increased with laundering and wear, consistent with the increase in yarn count and fabric weight.
For gowns, the flammability met the criterion for char length. No specimen failed the flammability standard or burned the entire length. Laundering significantly influenced the char lengths of the pajamas. Only two samples failed the criterion for char length, and all three specimens of these two samples burned the entire length. In conclusion, the l00 percent cotton FR pajamas had good flame resistance, but some failures were noted. Polyester/matrix blend had good flame resistance with an average char length of 3.8 cm.