Processing and properties of high-speed melt spun and drawn poly(L-lactide) fibers
High-speed melt spun poly(L-lactic acid) fibers were prepared at take-up velocities up to 5000 m/min. Some fibers were further processed by hot-drawing. PLLA samples were investigated with respect to molecular weight, percent D-isomer content, mass throughput and draw temperature. Highest mechanical properties were recorded for PLA-2 (Mw = 221,500) with a mass throughput of 0.72 g/min. Maximum Young's modulus and tensile strength values were 7.4 GPa and 392 MPa, respectively. Crystallinity and birefringence increased as a function of take-up velocity up to a maximum. A small decrease in these values was observed at the highest take-up speeds. Lower molecular weight PLLA attained maximum values at higher take-up velocities than the higher molecular weight sample. The addition of D-isomer led to the reduction of melting temperature, crystallinity and birefringence and as a result mechanical properties. Increasing mass throughput caused maximum physical properties to be lower and higher take-up velocities were necessary to reach them. Hot-drawing the fibers produced improvements in physical properties; although degradation and increased mass throughput most likely lowered overall values.
Thesis2001W55.pdf
5.44 MB
Adobe PDF
45667a06fdaaadeb5aa61792b96d93af