Kinetic properties of thin film solid solution gold (calcium) alloys prepared by simultaneous vapor deposition
Solid solution alloys of gold and calcium are very difficult to prepare by normal metallurgical techniques. I have simultaneously deposited the two metals from separately controlled deposition sources, and quenched the alloy from the vapor phase by allowing it to come into contact with a cooled glass substrate. Samples have been produced while maintaining the substrate at both liquid nitrogen and room temperature. X-ray diffraction measurements on all samples indicate a shift in the lattice parameter in a direction negative to that expected from Vegard's law. For small concentrations of calcium in gold the diffraction measurements indicate an f.c.c. crystal structure with δa/a = -.0010 ± .0002 per atomic percent of calcium. For higher concentrations amorphous phases are observed which anneal out exponentially with time, eventually reverting to the f.c.c. structure. In samples prepared on the cooled substrate, a reduction in the initial intensity and a corresponding broadening in the width of the 111 peak has been observed. These effects anneal out at temperatures as low as 100°C. Kinetics of the annealing process for isothernal and isochronal annealing are examined.
Thesis78K452.pdf
2.12 MB
Adobe PDF
8fc854b270473bf2cf5b8d5e8dc59020